PFA Heat Shrink Tube Supplier
HOME / PRODUCT / Heat Shrink Tube / PFA Heat Shrink Tube
Heat Shrink Tube

PFA Heat Shrink Tube

PFA heat shrink tubing is a heat shrinkable insulation material made of high-performance fluoroplastic perfluoroalkoxy resin (PFA for short). It has the functions of high-temperature shrinkage, soft flame retardancy, insulation and corrosion resistance. It is widely used in many fields due to its good performance.

Advantages:

  • Good lubricity;
  • Good biocompatibility;
  • Good dielectric insulation;
  • Good chemical resistance;
  • Good weather resistance;
  • Operating temperature range: -40℃ to 260℃;
  • Shrinkage temperature: 180℃ to 250℃.

  • SPECIFICATIONS
  • APPLICATIONS
  • CONTACT US
  • PFA Heat Shrink Tube Specifications
     Expanded ID 0.70mm-12.7mm
     Wall Thickness 0.10mm - 0.30mm
     Length Standard: 125 cm (minimum)
    Custom Cutting:
    Maximum straight length: 2500mm
    Longer lengths possible for some sizes
    Minimum: 0.5mm or less
     Colors Standard:
    • Optically clear
    • Other colors may be available upon request
     Temperature Range Operating Temp:-40℃ - 260℃
    Recovery Temp: 180℃ - 250℃
     Shrinkage/Sizing Shrink Ratios: 1.3/1.6 times
     Electrical Properties Dielectric strength: ≥300KV/mm
    Dielectric constant: 60Hz,2.0-2.1
    Volume resistivity: >10
    18ohm-cm
     Sterilization EtO
     Biocompatibility Biocompatible (GB/T 16886)

  • It is widely used in cable insulation protection and conduit covering of medical devices, heat exchangers and steam piping in power plants, high-purity reagent transportation and various corrosive medium transportation pipes in the chemical industry, various frequency wire and cable sheaths in the communication industry, semiconductor manufacturing equipment and other industries.

  • Message Feedback
EXPLORE OUR FEATURED PRODUCTS
Excellent product with exquisite craftsmanship
  • Multi-lumen Tubing Multi-lumen Tubing
    Multi-lumen tubing is designed with multiple channels within a single tube, featuring various external shapes and lumen configurations, to allow simultaneous access for guidewires, medications, gases, and other substances. Our rich production experience and good extrusion technology can ensure the stability of our Multi-lumen Tubing and provide support for your project.
    READ MORE
  • Balloon Tubing Balloon Tubing
    Balloon tubing is primarily used for the processing of the balloon body in balloon dilatation catheters (commonly referred to as balloons), serving as the core and critical component of balloon tubing. With extensive extrusion experience, we are capable of consistently providing you with balloon tubing that features tight tolerances and good mechanical properties, meeting your requirements.
    READ MORE
  • Medical Multi-layer Tubing Medical Multi-layer Tubing
    The medical multi-layer tubing is constructed from two or more layers of materials, each selected based on specific criteria such as strength, flexibility, chemical resistance, and impermeability. The inner and outer layers may consist of different materials, with the inner layer prioritizing biocompatibility and the outer layer providing additional strength or protection.
    READ MORE
  • TPU Radiopaque Tubing TPU Radiopaque Tubing
    The application of TPU materials in radiopaque tubing is becoming more and more widespread, bringing new breakthroughs in fields such as medical diagnosis.
    READ MORE
  • Ultra Thin Wall Medical Tubing Ultra Thin Wall Medical Tubing
    Ultra thin wall medical tubing is distinguished by its slender wall thickness, precise inner diameter, diverse material options, and good biocompatibility. The thin-wall design of these tubes allows for sufficient strength while reducing irritation and damage to internal tissues, significantly reducing the risk of infection and complications. Moreover, the precise control of the inner diameter ensures stable and efficient fluid transport, and the variety of materials caters to the complex requirements of various medical scenarios.
    READ MORE
  • Braid Reinforced Tubing Braid Reinforced Tubing
    The braid-reinforced tubing is crafted through co-extrusion or reflow processes, embedding metal or fiber braided structures between two layers of material. This innovative design significantly enhances the tube's burst pressure resistance, column strength, and torque transmission. The braiding angle, coverage, and the dimensions, shape, and strength of the reinforcing materials are critical in determining the performance of the tubes. We pride ourselves on producing mesh-braided tubes with high precision and good mechanical properties, which can be tailored to meet your specific requirements.
    READ MORE
  • Coil Reinforced Tubing Coil Reinforced Tubing
    Coil Reinforced Tubing is manufactured by incorporating spring coils between two layers of material through co-extrusion or reflow processes, resulting in composite tubing with enhanced pressure resistance, fold resistance, and torsional control. We are committed to meeting our clients' specific requirements by customizing product development and production accordingly. The coil reinforced tubing is characterized by their good smoothness, strong compatibility, and good support.
    READ MORE
  • Steerable Sheath Steerable Sheath
    The steerable sheath is a distal adjustable bending sheath that can be adjusted in vitro so that the distal end of the sheath can be bent to different angles in the patient. It has precise pointing and can adapt to different anatomical structures.
    READ MORE
  • High Pressure Braided Tubing High Pressure Braided Tubing
    High-Pressure Braided Tubing, or High-Pressure Monitoring Tubing, is used to inject contrast media and other medical solutions during PTCA, PCI procedures or angioplasty procedures.
    READ MORE
  • Micro Catheter Micro Catheter
    Micro catheters are small-sized reinforced catheters, usually with an outer diameter of less than 1 mm. They are often used in minimally invasive surgeries of complex blood vessels in the human body and can enter tiny blood vessels and cavities in the human body, such as nerve vessels, to achieve precise treatment. Our micro catheters have good flexibility, maneuverability and biocompatibility, and can well meet the needs of clinical operations.
    READ MORE
  • Medical Polyimide Tubing Medical Polyimide Tubing
    Medical Polyimide Tubing exhibits good strength and wear resistance, maintaining its performance even at small dimensions. For medical surgical applications that demand additional lubricity, PI/PTFE composite materials offer a lower coefficient of friction, thereby reducing the surface resistance of the tubing. By combining the unique properties of PI and PTFE, the tubing ensures a sufficiently smooth inner wall, while the PI component enhances the structural support of the entire tube, effectively preventing deformation.
    READ MORE